Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00100 GPa | 0.145 ksi | BS4370, part 4, method 14 |
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |