Polymer Property : Izod Impact, Unnotched = 9.93 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.30 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
9.93 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PA 1406
PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 ..
Izod Impact, Unnotched 5.30 J/cm

@Temperature 23.0 °C
9.93 ft-lb/in

@Temperature 73.4 °F
ASTM D4812
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers