Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.80 J/cm

@Thickness 4.00 mm,
Temperature -20.0 °C
16.5 ft-lb/in

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PC 1431
PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Izod Impact, Unnotched 8.80 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
16.5 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PC 1431
PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..