Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.70 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
5.06 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |