Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.00 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
9.37 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Izod Impact, Unnotched | 5.00 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
9.37 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Izod Impact, Unnotched | 5.00 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Unnotched | 5.00 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
9.37 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Izod Impact, Unnotched | 5.00 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |