Polymer Property : Izod Impact, Unnotched = 20.6 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 11.0 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Unnotched 11.0 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..