Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.25 J/cm @Thickness 12.7 mm |
2.35 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP310HT Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness.. |