Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.00 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
11.2 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1380 PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR.. |
|||
Izod Impact, Unnotched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D 4812 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |