Polymer Property : Izod Impact, Unnotched = 1.28 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.28 J/cm

@Thickness 12.7 mm
2.40 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP347 Cotton Fabric
Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1..
Izod Impact, Unnotched 1.28 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.40 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Unnotched 1.28 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.40 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.