Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.981 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Izod Impact, Unnotched >= 0.981 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
>= 1.84 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ISO 180
LG Chemical EM500 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Izod Impact, Unnotched >= 0.981 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
>= 1.84 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ISO 180
LG Chemical EM500A Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Izod Impact, Unnotched >= 0.981 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
>= 1.84 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ISO 180
LG Chemical EM505 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical ER451 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LG703W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical ER461 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
Izod Impact, Unnotched 0.981 J/cm

@Thickness 6.40 mm,
Temperature -20.0 °C
1.84 ft-lb/in

@Thickness 0.252 in,
Temperature -4.00 °F
ASTM D256
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -20.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -4.00 °F
ASTM D256
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
Izod Impact, Unnotched 0.981 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical XR401F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical