Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.459 J/cm @Thickness 12.7 mm |
0.860 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |