Mechanical Properties Metric English Comments
Flexural Modulus 8.50 GPa

@Temperature 200 °C
1230 ksi

@Temperature 392 °F
ISO 178
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree..
Flexural Modulus 8.50 GPa

@Temperature 200 °C
1230 ksi

@Temperature 392 °F
ISO 178
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber
Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional ..
Flexural Modulus 8.50 GPa

@Temperature 23.0 °C
1230 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 8.50 GPa

@Temperature 23.0 °C
1230 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..