Mechanical Properties Metric English Comments
Flexural Modulus 72.19 GPa

@Temperature 23.0 °C
10470 ksi

@Temperature 73.4 °F
Press Cured;
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form
Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel