Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0500 GPa @Temperature -40.0 °C |
7.25 ksi @Temperature -40.0 °F |
ISO 178 |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |