Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.80 GPa @Temperature 23.0 °C |
696 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |