Flexural Modulus 43.0 GPa

@Temperature 23.0 °C
6240 ksi

@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D790
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel