Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 5800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 40.0 GPa

@Temperature 23.0 °C
5800 ksi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D790
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA
Fiber Designation: C193PW, Plain weaveInformation provided by HexCel
Flexural Modulus 40.0 GPa

@Temperature 90.0 °C
5800 ksi

@Temperature 194 °F
0º, Conditioning: 23°C; ASTM D790
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel
Copyright © lookpolymers.com All Rights Reserved