Flexural Modulus 5.40 GPa

@Temperature -40.0 °C
783 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.40 GPa

@Temperature 23.0 °C
783 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.40 GPa

@Temperature 80.0 °C
783 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.40 GPa

@Temperature 23.0 °C
783 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.40 GPa

@Temperature 80.0 °C
783 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.40 GPa

@Temperature 80.0 °C
783 ksi

@Temperature 176 °F
Practical Use; ASTM-D790
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..