Mechanical Properties Metric English Comments
Flexural Modulus 5.30 GPa

@Temperature 23.0 °C
769 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 5.30 GPa

@Temperature 23.0 °C
769 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.30 GPa

@Temperature 177 °C
769 ksi

@Temperature 351 °F
Autoclave Cured; [90°]16; Wet condition
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel
Flexural Modulus 5.30 GPa

@Temperature 177 °C
769 ksi

@Temperature 351 °F
T300 (6K); [90°]16; Wet Condition
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel