Flexural Modulus 4.48 GPa

@Temperature -40.0 °C
650 ksi

@Temperature -40.0 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers