Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.66 GPa @Temperature 23.0 °C |
531 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 3.66 GPa @Temperature 23.0 °C |
531 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Flexural Modulus | 3.66 GPa @Temperature -40.0 °C |
531 ksi @Temperature -40.0 °F |
ASTM D790 |
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |