Polymer Property : Flexural Modulus = 263.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.819 GPa

@Temperature 260 °C
263.8 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L