Polymer Property : Flexural Modulus = 22.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 22.8 GPa

@Temperature 93.3 °C
3300 ksi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Flexural Modulus 22.8 GPa

@Temperature 23.9 °C
3300 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..
Flexural Modulus 22.8 GPa

@Temperature 23.9 °C
3300 ksi

@Temperature 75.0 °F
Wet (2 hour water boil); ASTM D790
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..