Polymer Property : Flexural Modulus = 21.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.145 GPa

@Temperature -40.0 °C
21.0 ksi

@Temperature -40.0 °F
ISO 178
DuPont Performance Polymers Hytrel® 3078FG TPC-ET  (Unverified Data**)
Hytrel® 3078FG is a high performance thermoplastic elastomer with food compliance specificity.Information provided by DuPont Performance Polymers