Polymer Property : Flexural Modulus = 2.4463 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.4463 GPa

@Temperature 23.0 °C
354.80 ksi

@Temperature 73.4 °F
ASTM D790
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L