Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.9 GPa @Temperature 23.9 °C |
2300 ksi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |