Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.823 GPa @Temperature 23.0 °C |
119 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |