Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.683 GPa @Temperature 23.0 °C |
1114 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66
(Unverified Data**) Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im.. |