Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.7 GPa @Temperature 93.3 °C |
1700 ksi @Temperature 200 °F |
Dry; Post-Cure; ASTM D790 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Flexural Modulus | 11.7 GPa @Temperature 23.0 °C |
1700 ksi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Flexural Modulus | 11.7 GPa @Thickness 0.500 mm, Temperature 22.0 °C |
1700 ksi @Thickness 0.0197 in, Temperature 71.6 °F |
secant; ASTM D790-1 |
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Flexural Modulus | 11.7 GPa @Temperature 23.0 °C |
1700 ksi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Flexural Modulus | 11.7 GPa @Temperature -40.0 °C |
1700 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.6%); ASTM-D790 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 11.7 GPa @Thickness 0.500 mm, Temperature 22.0 °C |
1700 ksi @Thickness 0.0197 in, Temperature 71.6 °F |
Secant; ISO 178 |
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo.. |
|||
Flexural Modulus | 11.7 GPa @Temperature 23.0 °C |
1700 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |