Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.3 GPa @Temperature 232 °C |
1490 ksi @Temperature 450 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Flexural Modulus | 10.3 GPa @Thickness 1.57 mm |
1500 ksi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Flexural Modulus | 10.3 GPa @Thickness 1.57 mm |
1500 ksi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Flexural Modulus | 10.3 GPa @Thickness 1.57 mm |
1500 ksi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Flexural Modulus | 10.3 GPa @Thickness 1.57 mm |
1500 ksi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Flexural Modulus | 10.3 GPa @Thickness 1.57 mm |
1500 ksi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Flexural Modulus | 10.3 GPa @Thickness 1.57 mm |
1500 ksi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Flexural Modulus | 10.3 GPa @Temperature 232 °C |
1490 ksi @Temperature 450 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |