Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.50 GPa

@Temperature 23.0 °C
218 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Crastin® ST820 BK503 PBT  (Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 1.50 GPa

@Temperature 23.0 °C
218 ksi

@Temperature 73.4 °F
50%RH; ASTM D790
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Flexural Modulus 1.50 GPa

@Temperature 23.0 °C
218 ksi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Flexural Modulus 1.50 GPa

@Temperature 80.0 °C
218 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.7%); ASTM-D790
Toyobo GLAMIDE® TY-145TZ Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.50 GPa

@Temperature 80.0 °C
218 ksi

@Temperature 176 °F
Practical Use (Water Absorption 1.7%); ASTM-D790
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.50 GPa

@Temperature 23.0 °C
218 ksi

@Temperature 73.4 °F
Practical Use; ASTM-D790
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..