Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.38 GPa @Temperature 23.0 °C |
200 ksi @Temperature 73.4 °F |
50%RH; ASTM D790 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |