Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0140 GPa @Temperature 100 °C |
2.03 ksi @Temperature 212 °F |
ISO 178 |
DuPont Performance Polymers Hytrel® 3078FG TPC-ET
(Unverified Data**) Hytrel® 3078FG is a high performance thermoplastic elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |