Polymer Property : Flexural Modulus = 0.00260 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.00260 GPa

@Temperature 150 °C
0.377 ksi

@Temperature 302 °F
ASTM D790
DuPont Performance Polymers VESPEL TP-8054 Polyimide
DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi..