Polymer Property : Gardner Impact = 9.49 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 9.49 J

@Temperature -5.56 °C
7.00 ft-lb

@Temperature 22.0 °F
ASTM D5420
Spartech PE4125 Reinforced High Density Polyethylene Compound
Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a..