Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 6.44 J @Temperature -30.0 °C |
4.75 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Washington Penn Medium Impact Copolymer 10% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |