Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 5.42 J @Temperature -5.56 °C |
4.00 ft-lb @Temperature 22.0 °F |
ASTM D5420 |
Spartech PE4325 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |