Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 4.00 J @Temperature -29.0 °C |
2.95 ft-lb @Temperature -20.2 °F |
6 m/s; ASTM D5420 |
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc.. |
|||
Gardner Impact | 4.00 J @Temperature -40.0 °C |
2.95 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |