Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
Gardner Impact | 37.0 J @Temperature 23.0 °C |
27.3 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |