Polymer Property : Gardner Impact = 15.3 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 20.8 J

@Temperature -30.0 °C
15.3 ft-lb

@Temperature -22.0 °F
ASTM D5420
Washington Penn Medium Impact Copolymer 30% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..