Polymer Property : Gardner Impact = 13.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 13.8 J

@Temperature -30.0 °C
10.2 ft-lb

@Temperature -22.0 °F
ASTM D5420
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Gardner Impact 13.8 J

@Temperature 23.0 °C
10.2 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Medium Impact Copolymer 30% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..