Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 18.1 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Medium Impact Copolymer 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |