Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 80.2 J @Thickness 3.20 mm, Temperature -40.0 °C |
59.2 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
Injection Molded, Total Energy; ASTM D3763 |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |