Mechanical Properties Metric English Comments
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA
High flow PPO+PA. Power distribution box applications.
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific)
High flow PPO+PA. Power distribution box applications.