Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |