Polymer Property : Dart Drop, Total Energy = 36.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 50.0 J

@Temperature -30.0 °C
36.9 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS
PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact
Dart Drop, Total Energy 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS
Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications.
Dart Drop, Total Energy 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific)
IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business.
Dart Drop, Total Energy 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Dart Drop, Total Energy 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® V3900WX PBT+PC
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Dart Drop, Total Energy 50.0 J

@Temperature -40.0 °C
36.9 ft-lb

@Temperature -40.0 °F
ASTM D3763
SABIC Innovative Plastics Valox® V3900WX PBT+PC
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Dart Drop, Total Energy 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Dart Drop, Total Energy 50.0 J

@Temperature -40.0 °C
36.9 ft-lb

@Temperature -40.0 °F
ASTM D3763
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.