Polymer Property : Dart Drop, Total Energy = 30.7 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 30.7 J

@Temperature -18.0 °C
22.6 ft-lb

@Temperature -0.400 °F
Peak Energy; ASTM D3763
Dow 500.00 Developmental Performance Polypropylene Polymer
D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applica..