Polymer Property : Dart Drop, Total Energy = 29.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 783.CD is a 31.4% VA copolymer that is suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and very low modulus. L..