Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Dart Drop, Total Energy | 27.0 J @Temperature -30.0 °C |
19.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Dart Drop, Total Energy | 27.0 J @Temperature 22.8 °C |
19.9 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |