Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 28.4 J @Thickness 3.20 mm, Temperature 0.000 °C |
20.9 ft-lb @Thickness 0.126 in, Temperature 32.0 °F |
6.7 m/sec, Fully Ductile; ASTM D3763 |
Styron INSPIREâ„¢ DTF8000 ES Compounded Polypropylene Overview: INSPIREâ„¢ TF 8000 ES is a superior scratch and mar resistant low gloss talc filled interior grad TPO exhibiting excellent low temperature ductility, high modulus and heat performance.M.. |